X-Ray Spectroscopy[1]
Revising author
-
Published:2019
Abstract
This article provides a detailed account of X-ray spectroscopy used for elemental identification and determination. It begins with an overview of the operating principles of X-ray fluorescence (XRF) spectrometer, as well as a comparison of the operating principles of wavelength-dispersive spectrometer (WDS) and energy-dispersive spectrometer (EDS). This is followed by a discussion on the mechanism and effects of X-ray radiation, X-ray emission, and X-ray absorption. The article then discusses components used, operation, and applications of WDS and EDS. Some of the factors and processes involved in sample preparation for XRF analysis are also included. The article further provides information...
Sign in
ASM members
Member Sign InS. Lampman, X-Ray Spectroscopy, Materials Characterization, Vol 10, 2019 ed., ASM Handbook, ASM International, 2019, p 337–361, https://doi.org/10.31399/asm.hb.v10.a0006645
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!