Differential Scanning Calorimetry[1]
By
Victoria Burt
Victoria Burt
ASM International
Revising author
Search for other works by this author on:
-
Published:2019
Abstract
Differential scanning calorimetry (DSC) is the most common thermal technique for polymer characterization. This article provides a detailed account of the various factors and processes involved in DSC. The discussion covers the equipment used, specimen preparation process, calibration requirements, data analysis, and provides examples of the applications and interpretation of DSC.
You do not currently have access to this chapter.
Citation
Victoria Burt, Differential Scanning Calorimetry, Materials Characterization, Vol 10, 2019 ed., ASM Handbook, ASM International, 2019, p 305–311, https://doi.org/10.31399/asm.hb.v10.a0006672
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Environmental and Chemical Effects
Characterization and Failure Analysis of Plastics
Material Jetting of Polymers
Additive Manufacturing Processes
Thermal Analysis
Composites
Failure Analysis of Transformer Brackets
Handbook of Case Histories in Failure Analysis
Failure Analysis of Epoxy Resin Encapsulant During a Long-Term Storage
Handbook of Case Histories in Failure Analysis
Characterization of Plastics in Failure Analysis
Characterization and Failure Analysis of Plastics
Powder Bed Fusion of Polymers
Additive Manufacturing Processes
Flammability Testing
Characterization and Failure Analysis of Plastics
Laboratory Testing
Protective Organic Coatings
Characterization of Thermosetting Resins and Polymers
Characterization and Failure Analysis of Plastics