Skip to Main Content
ASM Handbook

Heat Treating of Irons and Steels

Edited by
Jon L. Dossett
Jon L. Dossett
Consultant
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4D
ISBN electronic:
978-1-62708-168-9
Publication date:
2014
Book Chapter

Heat Treatment Problems Associated with Design and Steel Selection[1]

Published:
2014
Page range:
3 - 28
Publication history
October 30, 2014

Abstract

This article presents an overview of common heat treating problems arising due to poor part design, material incapabilities, difficult engineering requirements, incorrect heat treatment practice, and nonuniform quenching with emphasis on distortion and cracking of quenched and tempered steels. It provides useful information on selection of steels for heat treatment, and discusses the causes of residual stresses, distortion (size and shape), and size changes due to hardening and tempering. The article elucidates the control techniques for such distortions. It describes the importance of decarburizing, and discusses the problems caused by heating, cracking, quenching, typical steel grades, and design.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Heat Treatment Problems Associated with Design and Steel Selection", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal