Book Chapter

Hardenability Bands of Alloy Steels

Published:
2014
Page range:
552 - 562
Publication history
October 30, 2014

Abstract

This article is a comprehensive collection of graphs that present information on the hardenability bands of various grades of alloy steels. It also includes figures showing correlations of Jominy equivalent cooling rates, plots of end-quench bands of carbon steels, and logarithmic plots of relative hardenability of carbon steels.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Hardenability Bands of Alloy Steels", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal