Skip to Main Content
ASM Handbook

Heat Treating of Irons and Steels

Edited by
Jon L. Dossett
Jon L. Dossett
Consultant
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4D
ISBN electronic:
978-1-62708-168-9
Publication date:
2014
Book Chapter

Austenitizing and Typical Heat Treatment Temperatures for Steels

Published:
2014
Page range:
545 - 549
Publication history
October 30, 2014

Abstract

This article is a compilation of tables that present information on austenitizing temperatures for direct-hardening carbon and alloy steels, case depth of steels for different carburizing times and temperatures, typical heat treatments for case hardening of carbon and carburizing of alloy steels, as well as direct hardening of carbon steels and alloy steels.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Austenitizing and Typical Heat Treatment Temperatures for Steels", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal