Nitriding of Stainless Steels

By
Luiz Carlos Casteletti
Luiz Carlos Casteletti
University of São Paulo
Search for other works by this author on:
Amadeu Lombardi Neto
Amadeu Lombardi Neto
Federal Technological University of Parana-Londrina
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
Published:
2014
Page range:
418 - 438
Publication history
October 30, 2014

Abstract

Stainless steels are essential for the modern industrial civilization because of their corrosion resistance, especially in the chemical, petrochemical, and food industries. This article discusses the classification of the various types of stainless steels, including martensitic, ferritic, austenitic, duplex (ferritic-austenitic), and precipitation-hardening stainless steels. It presents a checklist of characteristics to be considered in selecting the proper type of stainless steel for a specific application. The article also outlines the need to promote the formation of an effective protective passive layer in stainless steels. It discusses hardness, fatigue and fretting properties, tribological properties, wear resistance, and corrosion-wear process of the S-phase layer. The article describes two thermochemical nitriding techniques of stainless steels: plasma-assisted nitriding techniques and non-plasma assisted nitriding processes. It also describes the difficulties in stainless steel nitriding/carburizing.

You do not currently have access to this content.
Don't already have an account? Register

Luiz Carlos Casteletti, Amadeu Lombardi Neto, George E. Totten, 2014. "Nitriding of Stainless Steels", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal