Heat Treatment of Malleable and Compacted-Graphite Irons

Published:
2014
Page range:
522 - 526
Publication history
October 30, 2014

Abstract

This article focuses on heat treatment of malleable and compacted-graphite irons to produce ferritic and pearlitic malleable irons. It describes the heat treatment cycles of malleable iron, including martempering, tempering, bainitic heat treatment, and surface hardening. The article provides information on the mechanical and physical properties of compacted-graphite irons, which are determined by the graphite shape and the pearlite/ferrite ratio.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Heat Treatment of Malleable and Compacted-Graphite Irons", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal