Steel Hardness Conversions

Published:
2014
Page range:
577 - 582
Publication history
October 30, 2014

Abstract

Hardness conversions are empirical relationships that are defined by conversion tables limited to specific categories of materials. This article is a comprehensive collection of tables that list hardness conversion formulas. Approximate Rockwell B and C hardness conversion numbers for nonaustenitic steels, and approximate equivalent hardness numbers for Brinell and Vickers (diamond pyramid) hardness numbers for steels are provided.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Steel Hardness Conversions", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal