Skip to Main Content
ASM Handbook

Heat Treating of Irons and Steels

Edited by
Jon L. Dossett
Jon L. Dossett
Consultant
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4D
ISBN electronic:
978-1-62708-168-9
Publication date:
2014
Book Chapter

Steel Cross Reference to AISI/SAE Designations

Published:
2014
Page range:
572 - 576
Publication history
October 30, 2014

Abstract

This article is a compilation of tables that present information on cross-referencing of steel designations that are followed in France, Germany, Italy, Japan, Sweden, and Britain to AISI/SAE.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Steel Cross Reference to AISI/SAE Designations", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal