Skip to Main Content
ASM Handbook

Heat Treating of Irons and Steels

Edited by
Jon L. Dossett
Jon L. Dossett
Consultant
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4D
ISBN electronic:
978-1-62708-168-9
Publication date:
2014
Book Chapter

Heat Treating of Precipitation-Hardenable Stainless Steels and Iron-Base Superalloys[1]

By
Lin Li
Lin Li
Shanghai University
Search for other works by this author on:
Published:
2014
Page range:
397 - 417
Publication history
October 30, 2014

Abstract

Precipitation hardening is a hardening mechanism found in various steels and alloy systems, such as nickel-, cobalt-, titanium-, copper-, and iron-base alloys. This article provides a brief description of precipitation hardening process, furnace equipment, surface-related problems, and protective atmospheres used in heat treatment of iron-base precipitation-hardenable (PH) superalloys. It focuses on various factors to be considered in heat treating of PH stainless steels: cleaning prior to heat treatment, furnace atmospheres, time-temperature cycles, variations in cycles, and scale removal after heat treatment. The article describes the mechanical properties, solution treatment, and aging treatment for many martensitic PH alloys, including: Alloy 17-4 PH, Alloy 13-8 Mo, Alloy 15-5 PH, Custom 450, and Custom 455; as well as semiaustenitic PH stainless steels such as Alloy 17-7 PH, Alloy PH 15-7 Mo, AM-350, Pyromet 350, AM-355, and Pyromet 355; austenitic PH stainless steel, A-286; cast PH stainless steels; and iron-nickel PH superalloys.

You do not currently have access to this content.
Don't already have an account? Register

Lin Li, 2014. "Heat Treating of Precipitation-Hardenable Stainless Steels and Iron-Base Superalloys", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal