Book Chapter

Heat Treating of High-Alloy White Cast Irons[1]

Published:
2014
Page range:
527 - 535
Publication history
October 30, 2014

Abstract

High-alloyed white cast irons are an important group of materials whose production must be considered separately from that of ordinary types of cast irons. The metallic matrix supporting the carbide phase in the high-alloy white cast irons can be adjusted by alloy content and heat treatment to develop proper balance between resistance to abrasion and toughness needed to withstand repeated impact. This article provides a brief discussion on the heat treatment, mechanical properties, and chemical compositions of high-alloy white cast irons such as nickel-chromium white irons and high-chromium white irons.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Heat Treating of High-Alloy White Cast Irons", Heat Treating of Irons and Steels, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal