Materials for Heat-Treating Furnace Parts, Trays, and Fixtures[1]

Published:
2014
Page range:
242 - 252
Publication history
August 31, 2014

Abstract

This article reviews high-temperature corrosion of furnace parts used in heat-treating furnaces. It provides a comparison of cast and wrought materials in the context of their general considerations, advantages, and applications. The article provides information on the heat-resistant alloys used for parts that go through the furnaces, including trays, fixtures, conveyor chains and belts, and quenching fixtures and parts, and the parts that remain in the furnace such as combustion tubes, radiant tubes, burners, thermowells, roller and skid rails, baskets, pots, retorts, muffles, and drive and idler drums. The article also reviews the material characteristics of silicon/silicon carbide composite and reaction-bonded silicon carbide as used in radiant tubes.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Materials for Heat-Treating Furnace Parts, Trays, and Fixtures", Steel Heat Treating Technologies, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal