Skip to Main Content
ASM Handbook

Steel Heat Treating Technologies

Edited by
Jon L. Dossett
Jon L. Dossett
Consultant
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4B
ISBN electronic:
978-1-62708-166-5
Publication date:
2014
Book Chapter

Guide to Furnace Atmospheres

Published:
2014
Page range:
469 - 471
Publication history
August 31, 2014

Abstract

This article describes the effects of furnace atmospheric elements on steels. These elements are air, water vapor, molecular nitrogen, carbon dioxide, and carbon monoxide. The article provides useful information on six groups of commercially important prepared atmospheres classified by the American Gas Association on the basis of method of preparation or on the original constituents employed. These groups are designated and defined as follows: Class 100, exothermic base; Class 200, prepared nitrogen base; Class 300, endothermic base; Class 400, charcoal base; Class 500, exothermic-endothermic base; and Class 600, ammonia base. These are subclassified and numerically designated to indicate variations in the method by which they are prepared. The article also contains a table that lists significant furnace atmospheres and their typical applications.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Guide to Furnace Atmospheres", Steel Heat Treating Technologies, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal