Skip to Main Content
ASM Handbook

Steel Heat Treating Technologies

Edited by
Jon L. Dossett
Jon L. Dossett
Consultant
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4B
ISBN electronic:
978-1-62708-166-5
Publication date:
2014
Book Chapter

Steel Heat Treating Process Control—An Introduction

Published:
2014
Page range:
3 - 19
Publication history
August 31, 2014

Abstract

The heat treatment of steel involves a number of processes (such as stress relieving, normalizing, annealing etc) to condition the microstructure and obtain desired properties. This article discusses typical heat treating process control procedures for carbon and low-alloy steels, as well as the importance of time, and temperature control in heat treatment. Temperature Uniformity Survey, a testing procedure intended to map variations in temperature throughout the furnace work zone, helps in precise control of temperature. The article focuses on the measuring instruments used to determine gas pressure, vacuum level, gas flow, and gas composition. It focuses on their measuring quenchant characteristics, including bulk temperature, viscosity, composition, and cooling efficiency. The article describes the procedures for detecting variability in the incoming product. It presents, through an example, the general application of design of experiments techniques to locate and tune vital process parameters. The devices used in the control process of mechanical components are also reviewed.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Steel Heat Treating Process Control—An Introduction", Steel Heat Treating Technologies, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal