Skip to Main Content
ASM Handbook

Steel Heat Treating Technologies

Edited by
Jon L. Dossett
Jon L. Dossett
Consultant
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4B
ISBN electronic:
978-1-62708-166-5
Publication date:
2014
Book Chapter

Quench Factor Characterization of Quenchants for Hardening of Steel

By
R.L.S. Otero
R.L.S. Otero
Universidade de São Paulo
,
Brazil
Search for other works by this author on:
W.R. Otero
W.R. Otero
Tecumseh do Brasil Ltda.
,
Brazil
Search for other works by this author on:
L.C.F. Canale
L.C.F. Canale
Universidade de São Paulo
,
Brazil
Search for other works by this author on:
G.E. Totten
G.E. Totten
Portland State University
Search for other works by this author on:
Published:
2014
Page range:
304 - 309
Publication history
August 31, 2014

Abstract

Successful hardening depends on the hardenability of steel composition, the geometry of parts, the quenching system, and on the heat treating process used. This article provides a brief overview of the computation and use of quench factor analysis (QFA) to quantify as-quenched hardness for carbon and low-alloy steels. As a single-value parameter alternative to Grossmann H-values, QFA is a potential method to qualify a quenching medium or process or to effectively monitor variation of quench severity due to either the quenchant or the system. The article describes the procedures for experimentally determining the quench factors by using a type 304 austenitic stainless steel probe. Typical examples of the utilization of QFA for quenchant characterization are provided. The article also describes the methods for experimentally generating time-temperature-property curves.

You do not currently have access to this content.
Don't already have an account? Register

R.L.S. Otero, W.R. Otero, L.C.F. Canale, G.E. Totten, 2014. "Quench Factor Characterization of Quenchants for Hardening of Steel", Steel Heat Treating Technologies, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal