Skip to Main Content
ASM Handbook

Materials Characterization

Edited by
Ruth E. Whan
Ruth E. Whan
Sandia National Laboratories
Search for other works by this author on:
ASM International
Volume
10
ISBN electronic:
978-1-62708-178-8
Publication date:
1986
Book Chapter

Optical Metallography

By
M.R. Louthan, Jr.
M.R. Louthan, Jr.
Department of Materials Engineering, Virginia Polytechnic Institute and State University
Search for other works by this author on:
Published:
1986
Page range:
299 - 308

Abstract

Optical metallography, one of the most common materials characterization techniques, uses visible light to magnify structural features of interest. This article discusses the use of optical methods to evaluate micro and macrostructure and relate it to process conditions and material behavior. It covers the steps involved in sample preparation, including sectioning, mounting, grinding, polishing, and etching, and presents several examples of macro and microanalysis on various metals and alloys.

You do not currently have access to this content.
Don't already have an account? Register

M.R. Louthan, Jr., 1986. "Optical Metallography", Materials Characterization, Ruth E. Whan

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal