Raman Spectroscopy

By
Jeanne E. Pemberton
Jeanne E. Pemberton
Department of Chemistry, University of Arizona
Search for other works by this author on:
Anita L. Guy
Anita L. Guy
Department of Chemistry, University of Arizona
Search for other works by this author on:
Published:
1986
Page range:
126 - 138

Abstract

This article introduces the principles of Raman spectroscopy and the representative materials characterization applications to which Raman spectroscopy has been applied. It includes a discussion of light-scattering fundamentals and a description of the experimental aspects of the technique. Emphasis has been placed on the different instrument approaches that have been developed for performing Raman analyses on various materials. The applications presented in the article reflect the breadth of materials characterization uses for Raman spectroscopy and highlight the analysis of bulk material and of surface and near-surface species.

You do not currently have access to this content.
Don't already have an account? Register

Jeanne E. Pemberton, Anita L. Guy, 1986. "Raman Spectroscopy", Materials Characterization, Ruth E. Whan

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal