Book Chapter

Nuclear Magnetic Resonance

By
L.H. Bennett
L.H. Bennett
National Bureau of Standards
Search for other works by this author on:
L.J. Swartzendruber
L.J. Swartzendruber
National Bureau of Standards
Search for other works by this author on:
Published:
1986
Page range:
277 - 286

Abstract

Nuclear magnetic resonance (NMR) is a form of radio frequency spectroscopy based on interactions between nuclear magnetic dipole or electric quadrupole moments and an applied magnetic field or electric-field gradient. This article provides an overview of the fundamental principles of nuclear magnetic resonance with emphasis on nuclei properties, the basic equation of nuclear magnetic resonance, the classical theory of nuclear magnetization, line broadening, and measurement sensitivity. It describes the pulse-echo method for observing NMR. The article provides useful information on ferromagnetic nuclear resonance and nuclear quadrupole resonance, and illustrates the experimental arrangement of NMR with a block diagram. It also presents several application examples.

You do not currently have access to this content.
Don't already have an account? Register

L.H. Bennett, L.J. Swartzendruber, 1986. "Nuclear Magnetic Resonance", Materials Characterization, Ruth E. Whan

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal