Skip to Main Content
ASM Handbook

Aluminum Science and Technology

Edited by
Kevin Anderson, FASM
Kevin Anderson, FASM
Mercury Marine
Search for other works by this author on:
;
John Weritz
John Weritz
Aluminum Association
Search for other works by this author on:
;
J. Gilbert Kaufman, FASM
J. Gilbert Kaufman, FASM
Kaufman Associates
Search for other works by this author on:
ASM International
Volume
2A
ISBN electronic:
978-1-62708-207-5
Publication date:
2018
Book Chapter

Cold Extrusion of Aluminum Alloys[1]

By
S. Lampman
S. Lampman
ASM International
Search for other works by this author on:
Published:
2018
Page range:
311 - 314
Publication history
November 22, 2018

Abstract

Cold extrusion is typically used to create near-net-shape products, such as fasteners and automotive components. Aluminum alloys are well suitable to cold (impact) extrusion. This article describes the tooling, dies, punches, and tool materials of equipment used for cold extrusion. Typical tool materials and their working hardnesses for the extrusion of aluminum are presented. The article reviews the preparation of aluminum slugs in terms of tolerance on slug volume, surface preparation, and lubricants. It concludes with a discussion on extruded parts, such as shallow cup-like parts, deep cup-like parts, and parts with complex shapes.

You do not currently have access to this content.
Don't already have an account? Register

S. Lampman, 2018. "Cold Extrusion of Aluminum Alloys", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM