Skip to Main Content
ASM Handbook

Aluminum Science and Technology

Edited by
Kevin Anderson, FASM
Kevin Anderson, FASM
Mercury Marine
Search for other works by this author on:
John Weritz
John Weritz
Aluminum Association
Search for other works by this author on:
J. Gilbert Kaufman, FASM
J. Gilbert Kaufman, FASM
Kaufman Associates
Search for other works by this author on:
ASM International
Volume
2A
ISBN electronic:
978-1-62708-207-5
Publication date:
2018
Book Chapter

Laser Beam Machining of Aluminum and Aluminum Alloys

By
Mangesh V. Pantawane
Mangesh V. Pantawane
University of North Texas
Search for other works by this author on:
Sameehan S. Joshi
Sameehan S. Joshi
University of North Texas
Search for other works by this author on:
Narendra B. Dahotre
Narendra B. Dahotre
University of North Texas
Search for other works by this author on:
Published:
2018
Page range:
519 - 541

Abstract

This article focuses on a variety of laser beam machining (LBM) operations of aluminum and its alloys, namely, laser cutting, laser drilling, laser milling, laser turning, laser grooving, laser scribing, laser marking, and laser micromachining. It presents different approaches for carrying out machining operations, laser processing parameters, efficiency and accuracy of the process, and the effect of laser processing parameters on the quality of the machined surface. The article provides an overview of the various conventional (chip forming) and nonconventional machining techniques employed for aluminum-based materials. A comparison of the various aspects of LBM with other non-conventional techniques is also presented. The article also describes the features of LBM techniques employed for aluminum and its alloys for different types of machining.

You do not currently have access to this content.
Don't already have an account? Register

Mangesh V. Pantawane, Sameehan S. Joshi, Narendra B. Dahotre, 2018. "Laser Beam Machining of Aluminum and Aluminum Alloys", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM