978-1-62708-207-5
Publication date:
2018
Book Chapter

Metallurgy Basics for Aluminum Surface Treatment

By
Jude Mary Runge
Jude Mary Runge
CompCote International, Inc.
Search for other works by this author on:
John Weritz
John Weritz
Aluminum Association
Search for other works by this author on:
Published:
2018
Page range:
555 - 567
Publication history
November 22, 2018

Abstract

This article discusses the properties of aluminum surface and the applications of aluminum alloys. It explains the effects of trace elements on aluminum alloys. The article considers microstructural development of aluminum in terms of the surface and explains how it will impact corrosion resistance and surface treatment. It describes the thermodynamics of equilibrium oxidation processes and non-equilibrium corrosion processes. The article provides a discussion on aluminum oxidation under atmospheric and dynamic conditions. It presents the potential/pH (Pourbaix) diagram for aluminum under atmospheric and dynamic conditions. The article also explains the polarization effects during the formation of stable aluminum oxide under dynamic conditions. It concludes with information on the designation system for aluminum finishes.

You do not currently have access to this content.
Don't already have an account? Register

Jude Mary Runge, John Weritz, 2018. "Metallurgy Basics for Aluminum Surface Treatment", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal