Skip to Main Content
ASM Handbook

Aluminum Science and Technology

Edited by
Kevin Anderson, FASM
Kevin Anderson, FASM
Mercury Marine
Search for other works by this author on:
John Weritz
John Weritz
Aluminum Association
Search for other works by this author on:
J. Gilbert Kaufman, FASM
J. Gilbert Kaufman, FASM
Kaufman Associates
Search for other works by this author on:
ASM International
Volume
2A
ISBN electronic:
978-1-62708-207-5
Publication date:
2018
Book Chapter

Adhesive Bonding[1]

By
Victoria Burt
Victoria Burt
Revising author
ASM International
Search for other works by this author on:
Published:
2018
Page range:
783 - 789
Publication history
November 22, 2018

Abstract

Adhesive bonding has been used more and more in automotive joining for a variety of components, including closures and structural modules. This article discusses the functions of adhesive-bonded joints, as well as the limitations and advantages of adhesive bonding. It describes the characteristics of an adhesive joint and reviews the surface preparation for adhesive bonding in terms of surface pretreatment, surface cleaning, chemical conversion coating, and primer coating. The article discusses the thermoplastic resins and thermosetting resins, as well as the factors to be considered in selecting an adhesive. It concludes with information on the testing of adhesive joints.

You do not currently have access to this content.
Don't already have an account? Register

Victoria Burt, 2018. "Adhesive Bonding", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal