Skip to Main Content
ASM Handbook

Aluminum Science and Technology

Edited by
Kevin Anderson, FASM
Kevin Anderson, FASM
Mercury Marine
Search for other works by this author on:
John Weritz
John Weritz
Aluminum Association
Search for other works by this author on:
J. Gilbert Kaufman, FASM
J. Gilbert Kaufman, FASM
Kaufman Associates
Search for other works by this author on:
ASM International
Volume
2A
ISBN electronic:
978-1-62708-207-5
Publication date:
2018
Book Chapter

Semisolid Metal Casting

By
Stephen P. Midson
Stephen P. Midson
The Midson Group, Inc. and Colorado School of Mines
Search for other works by this author on:
Published:
2018
Page range:
400 - 408
Publication history
November 22, 2018

Abstract

Semisolid casting is a near-net shape manufacturing process capable of producing thick- and thin-walled complex-shaped components having excellent mechanical and functional performance. This article begins with a discussion on the history of semisolid processing and the advantages claimed for semisolid casting. It describes the four notable processes used to produce semisolid castings: thixocasting, rheocasting, thixomolding, and wrought processes. Most commercial aluminum semisolid casters use either thixocasting or rheocasting. The article discusses the die design, process conditions, and simulation for semisolid casting. It concludes with a review of several components produced by each of the various semisolid casting processes.

You do not currently have access to this content.
Don't already have an account? Register

Stephen P. Midson, 2018. "Semisolid Metal Casting", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal