Skip to Main Content
ASM Handbook

Aluminum Science and Technology

Edited by
Kevin Anderson, FASM
Kevin Anderson, FASM
Mercury Marine
Search for other works by this author on:
John Weritz
John Weritz
Aluminum Association
Search for other works by this author on:
J. Gilbert Kaufman, FASM
J. Gilbert Kaufman, FASM
Kaufman Associates
Search for other works by this author on:
ASM International
Volume
2A
ISBN electronic:
978-1-62708-207-5
Publication date:
2018
Book Chapter

Reference Information

Published:
2018

Abstract

This article presents a summary of aluminum temper designations, and applicable aluminum alloys and product forms for temper designations used in the United States (ANSI H35.1), Europe (EN 515), and internationally (ISO 2107).

You do not currently have access to this content.
Don't already have an account? Register

2018. "Reference Information", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal