Skip to Main Content
ASM Handbook

Aluminum Science and Technology

Edited by
Kevin Anderson, FASM
Kevin Anderson, FASM
Mercury Marine
Search for other works by this author on:
John Weritz
John Weritz
Aluminum Association
Search for other works by this author on:
J. Gilbert Kaufman, FASM
J. Gilbert Kaufman, FASM
Kaufman Associates
Search for other works by this author on:
ASM International
Volume
2A
ISBN electronic:
978-1-62708-207-5
Publication date:
2018
Book Chapter

Machining and Mechanical Finishing

Published:
2018

Abstract

The horsepower requirements to cut various metal alloys provide an indication of the relative ease and cost of machining, but several other important factors include cutting tool material, chip formation, cutting fluids, cutting tool wear, surface roughness, and surface integrity. This article reviews these general machining factors as well as specific cutting tool and cutting parameters for the six basic chip-forming processes of turning, shaping, milling, drilling, sawing, and broaching. Best practices for each of the six chip-forming processes are suggested for optimized machining of aluminum alloys. The article lists the inherent disadvantages of machining processes that involve compression/shear chip formation. It discusses the machining of aluminum metal-matrix composites and nontraditional machining of aluminum, such as abrasive jet, waterjet, electrodischarge, plasma arc, electrochemical, and chemical machining.

You do not currently have access to this content.
Don't already have an account? Register

2018. "Machining and Mechanical Finishing", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal