Photography of Fractured Parts and Fracture Surfaces

By
Theodore M. Clarke
Theodore M. Clarke
J.I. Case Company
Search for other works by this author on:
Published:
1987
Page range:
78 - 90
Publication history
January 01, 1987

Abstract

This article discusses the preparation of photomacrographs of fracture surfaces. It provides useful information on the equipment used, such as view cameras, 35-mm single-lens-reflex cameras, and stereomicroscopes. The article describes the role of lenses, focusing, camera magnification, and selection of lens aperture in a microscopic system. It illustrates the lighting techniques employed in photography and highlights the use of different films. The article concludes with a list of auxiliary equipment used in fracture surface photography.

You do not currently have access to this content.
Don't already have an account? Register

Theodore M. Clarke, 1987. "Photography of Fractured Parts and Fracture Surfaces", Fractography

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal