Preparation and Preservation of Fracture Specimens

By
Richard D. Zipp
Richard D. Zipp
J.I. Case Company
Search for other works by this author on:
E. Philip Dahlberg
E. Philip Dahlberg
Metallurgical Consultants, Inc.
Search for other works by this author on:
Published:
1987
Page range:
72 - 77
Publication history
January 01, 1987

Abstract

Fracture surfaces are fragile and subject to mechanical and environmental damage that can destroy microstructural features. This article discusses the importance of care and handling of fractures and the factors that need to be considered during the preliminary visual examination. It describes the procedures for sectioning a fracture and opening secondary cracks as well as the effect of nondestructive inspection on subsequent evaluation. The article provides information on the most common techniques for cleaning fracture surfaces. These techniques are dry air blast cleaning, replica stripping, organic-solvent cleaning, water-base detergent cleaning, cathodic cleaning, and chemical-etch cleaning.

You do not currently have access to this content.
Don't already have an account? Register

Richard D. Zipp, E. Philip Dahlberg, 1987. "Preparation and Preservation of Fracture Specimens", Fractography

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal