Cast Aluminum Alloys: Atlas of Fractographs

Published:
1987
Page range:
405 - 413
Publication history
January 01, 1987

Abstract

This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of cast aluminum alloys and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the brittle fracture, microvoid coalescence, fatigue striations, and microstructure of these alloys. The components considered include fractured sand-cast carrier trays, broken extension-housing yokes, helicopter tail-rotor drive assemblies, fractured bell-crank fittings, chain-hoist hooks, and automotive connecting rods.

You do not currently have access to this content.
Don't already have an account? Register

1987. "Cast Aluminum Alloys: Atlas of Fractographs", Fractography

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal