This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of titanium alloys and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the fracture surface, fatigue crack growth, intergranular fracture, crack propagation, ductile overload fracture, dimpled rupture, microvoid coalescence, and quasi-cleavage fracture of these alloys.

You do not currently have access to this content.
Don't already have an account? Register

1987. "Titanium Alloys: Atlas of Fractographs", Fractography, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal