Precipitation-Hardening Stainless Steels: Atlas of Fractographs

Published:
1987
Page range:
370 - 374
Publication history
January 01, 1987

Abstract

This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of precipitation-hardening stainless steels and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the cup-and-cone tension-overload fracture, low-cycle and high-cycle fatigue fracture, fracture surface, brittle intergranular fracture, hydrogen embrittlement, and intergranular stress-corrosion cracking of stainless steel components of these steels. The components include high-pressure compressor parts, springs, deflector yokes of aircraft main landing gears, and aircraft engine mount beams.

You do not currently have access to this content.
Don't already have an account? Register

1987. "Precipitation-Hardening Stainless Steels: Atlas of Fractographs", Fractography, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal