Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Fusion Welding Processes

By
Howard Cary
Howard Cary
Hobart Brothers Company
Search for other works by this author on:
Published:
1993

Abstract

Shielded metal arc welding (SMAW), commonly called stick or covered electrode welding, is a manual welding process whereby an arc is generated between a flux-covered consumable electrode and a workpiece. This article discusses the advantages and limitations and applications of the SMAW process and describes the equipment used. It provides information on various coated electrodes used in the SMAW process, including mild and low-alloy steel-covered electrodes, stainless steel covered electrodes, and nickel and copper alloys covered electrodes. It reviews weld schedules and procedures, as well as the variations of the SMAW process. The article concludes with information on the special applications of the SMAW process and safety considerations.

You do not currently have access to this content.
Don't already have an account? Register

Howard Cary, 1993. "Fusion Welding Processes", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal