Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Brazing of Conventional Titanium Alloys[1]

By
Alexander E. Shapiro
Alexander E. Shapiro
Titanium Brazing, Inc.
Search for other works by this author on:
Published:
1993
Page range:
1 - 25
Publication history
March 30, 2017

Abstract

This article discusses the effects of brazing temperature and thermal treatment on structure and mechanical behavior of different classes of titanium base metals such as commercially pure (CP) titanium, alpha or near-alpha alloys, alpha-beta alloys, and beta alloys. The classification, properties, and potential heat treatment of titanium base alloys are presented in tables. The article provides information on brazed joints of titanium with carbon steels, as well as ceramics and graphite. It discusses the risks involved in titanium brazing, including erosion of base metal, brittle intermetallics, and low ductility. The article reviews induction and torch brazing, infrared brazing, diffusion brazing, and brazing by heating with ion bombardment. It concludes by describing the design criteria and limitations of brazing.

You do not currently have access to this content.
Don't already have an account? Register

Alexander E. Shapiro, 1993. "Brazing of Conventional Titanium Alloys", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal