Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Residual Stresses and Distortion

By
Koichi Masubuchi
Koichi Masubuchi
Massachusetts Institute of Technology
Search for other works by this author on:
Published:
1993
Page range:
1094 - 1102

Abstract

This article describes the formation of residual stresses and distortion, providing information on the techniques for measuring residual stresses. It presents a detailed discussion on the magnitude and distribution analysis of the residual stresses and distortion in weldments. The article briefly explains the effects of residual stresses and distortion on the brittle fracture and fatigue fracture of welded structures. It also provides information on the thermal treatments of weldments.

You do not currently have access to this content.
Don't already have an account? Register

Koichi Masubuchi, 1993. "Residual Stresses and Distortion", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal