Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Brazing of Ceramic and Ceramic-to-Metal Joints

By
A.J. Moorhead
A.J. Moorhead
Oak Ridge National Laboratory
Search for other works by this author on:
W.H. Elliott, Jr.
W.H. Elliott, Jr.
Oak Ridge National Laboratory
Search for other works by this author on:
H.-E. Kim
H.-E. Kim
Seoul National University
Search for other works by this author on:
Published:
1993
Page range:
948 - 960

Abstract

This article is intended to assist the development of procedures for the brazing of ceramic-to-ceramic or ceramic-to-metal joints for service under elevated temperatures, mechanical or thermal stresses, or corrosive atmospheres. It describes the factors considered in preparing a procedure for the brazing of graphitic materials.

You do not currently have access to this content.
Don't already have an account? Register

A.J. Moorhead, W.H. Elliott, Jr., H.-E. Kim, 1993. "Brazing of Ceramic and Ceramic-to-Metal Joints", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal