Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Brazing of Refractory and Reactive Metals

By
Roy I. Batista
Roy I. Batista
TRW, Inc.
Search for other works by this author on:
Published:
1993
Page range:
941 - 947

Abstract

This article provides a discussion on filler metal selection, brazing procedures, and brazing equipment for brazing refractory metals. These include molybdenum, tungsten, niobium, and tantalum, and reactive metals. Commercially pure and alpha titanium alloys, alpha-beta alloys, zirconium alloys, and beryllium alloys are some reactive metals discussed in the article.

You do not currently have access to this content.
Don't already have an account? Register

Roy I. Batista, 1993. "Brazing of Refractory and Reactive Metals", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards