Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Brazing of Stainless Steels

By
Matthew J. Lucas, Jr.
Matthew J. Lucas, Jr.
Revising author
General Electric Aircraft Engines
Search for other works by this author on:
Published:
1993
Page range:
911 - 923

Abstract

The quality of brazed stainless steel joints depends on the selection of the brazing process, process temperature, filler metal, and the type of protective atmosphere or flux. This article provides a detailed discussion on the applicability and brazeability of stainless steel and lays an emphasis on the selection of suitable filler metal, brazing processes, and its corresponding furnace atmosphere for brazing different grades of stainless steel. The types of brazing processes include torch brazing, furnace brazing in different atmospheres (dissociated ammonia, dry hydrogen, and vacuum atmosphere), dip brazing in salt bath, and high-energy-beam brazing. A complete list of the typical compositions and properties of standard brazing filler metals for brazing stainless steel is also provided.

You do not currently have access to this content.
Don't already have an account? Register

Matthew J. Lucas, Jr., 1993. "Brazing of Stainless Steels", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal