Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Shielding Gases for Welding[1]

By
Kevin A. Lyttle
Kevin A. Lyttle
Praxair, Inc.
Search for other works by this author on:
Published:
1993
Page range:
64 - 69

Abstract

The shielding gas used in a welding process has a significant influence on the overall performance of the welding system. This article discusses the basic properties of a shielding gas in terms of ionization potential, thermal conductivity, dissociation and recombination, reactivity/oxidation potential, surface tension, gas purity, and gas density. It describes the characteristics of the components of a shielding gas blend. The article discusses the selection of shielding gas for gas-metal arc welding (GMAW), gas-tungsten arc welding (GTAW), and plasma arc welding (PAW), as well as the influence of shielding gas on weld mechanical properties. It concludes with a discussion on flux-cored arc welding.

You do not currently have access to this content.
Don't already have an account? Register

Kevin A. Lyttle, 1993. "Shielding Gases for Welding", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal