Book Chapter

Composite-to-Metal Joining

By
Raymond E. Bohlmann
Raymond E. Bohlmann
McDonnell Douglas Aerospace-East
Search for other works by this author on:
Published:
1993
Page range:
1041 - 1047

Abstract

This article discusses the material combinations, design details, and fabrication processes considered in the adhesive bonding or melt-fuse interface (amorphous bond) bonding method of joining resin-matrix composites to metals.

You do not currently have access to this content.
Don't already have an account? Register

Raymond E. Bohlmann, 1993. "Composite-to-Metal Joining", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards