Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Brazing of Cast Irons and Carbon Steels

By
Ann Severin
Ann Severin
Lucas-Milhaupt, Inc.
Search for other works by this author on:
Published:
1993
Page range:
906 - 910

Abstract

Cast irons and carbon steels are brazeable materials, although the brazeability of cast iron is lower than that of carbon steel. The article provides a detailed discussion on the brazeability of different types of cast iron (malleable iron, ductile iron, and gray iron), carbon steels, and dissimilar metals. It describes the factors considered in the selection of filler-metal for cast iron and carbon steel brazing, such as temperature and environment, brazed joint design, heat source, and heat-treatment requirements. The article also discusses the basic considerations in cleaning and fixturing procedures, filler metal and flux/atmosphere feeding procedures, and the heating methods of cast iron and carbon steel brazing.

You do not currently have access to this content.
Don't already have an account? Register

Ann Severin, 1993. "Brazing of Cast Irons and Carbon Steels", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal