Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Introduction to the Selection of Nonferrous Corrosion-Resistant Materials

By
S.J. Matthews
S.J. Matthews
Haynes International, Inc.
Search for other works by this author on:
Published:
1993
Page range:
585 - 585

Abstract

Improvement in the corrosion performance of a component or structure can be achieved through proper design, surface protection, proper material selection, or combinations of all three parameters. This is an introductory article on the selection of nonferrous corrosion-resistant materials.

You do not currently have access to this content.
Don't already have an account? Register

S.J. Matthews, 1993. "Introduction to the Selection of Nonferrous Corrosion-Resistant Materials", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards