Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Selection of Wrought Duplex Stainless Steels

By
David N. Noble
David N. Noble
ARCO Alaska, Inc.
Search for other works by this author on:
Published:
1993
Page range:
471 - 481

Abstract

This article provides information on the base material properties of wrought duplex stainless steels (DSS). These properties include microstructure, alloy grades, mechanical and physical properties, and corrosion resistance. The article reviews the applications and microstructural development of DSS. It describes the factors influencing welding and weldability of the DSS. These factors include preheating, postweld heat treatment, interpass temperature control, welding practices, welding procedure qualification, filler metal requirements, cracking behavior, and loss of properties. The article examines the applicable welding processes such as fusion welding and solid-state welding processes.

You do not currently have access to this content.
Don't already have an account? Register

David N. Noble, 1993. "Selection of Wrought Duplex Stainless Steels", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal