Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Influence of Welding on Steel Weldment Properties

By
C.C. Chen
C.C. Chen
Microalloying International, Inc.
Search for other works by this author on:
Abe Pollack
Abe Pollack
Microalloying International, Inc.
Search for other works by this author on:
Published:
1993
Page range:
416 - 428

Abstract

This article describes the fundamental and specific factors that control the properties of steel weldments in both the weld metal and heat-affected zone (HAZ) of carbon and low-alloy steels. It provides information on steel types and their weldability. The article also explains the influence of welding procedure factors on the weldment properties. These procedure factors include preheat temperature, interpass temperature, postweld heat treatment, and heat input.

You do not currently have access to this content.
Don't already have an account? Register

C.C. Chen, Abe Pollack, 1993. "Influence of Welding on Steel Weldment Properties", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards