Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Characterization and Modeling of the Heat Source

By
S.S. Glickstein
S.S. Glickstein
Westinghouse Electric Corporation
Search for other works by this author on:
E. Friedman
E. Friedman
Westinghouse Electric Corporation
Search for other works by this author on:
Published:
1993
Page range:
1141 - 1146

Abstract

This article briefly reviews the physical phenomena that influence the input-energy distribution. It discusses the several simplified and detailed heat source models used in the modeling of arc welding, high-energy-density welding, and resistance welding processes.

You do not currently have access to this content.
Don't already have an account? Register

S.S. Glickstein, E. Friedman, 1993. "Characterization and Modeling of the Heat Source", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal