Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Mechanical Properties of Soft-Interlayer Solid-State Welds[1]

By
R.S. Rosen
R.S. Rosen
Lawrence Livermore National Laboratory
Search for other works by this author on:
M.E. Kassner
M.E. Kassner
Oregon State University
Search for other works by this author on:
Published:
1993
Page range:
165 - 172

Abstract

Soft-interlayer solid-state welds that join stronger base metals have unique mechanical properties that are of fundamental interest and may be of critical importance to designers. This article discusses the mechanical properties of soft-interlayer solid-state welds and the implications of these behaviors to service stress states and environments. It describes the tensile loading of soft-Interlayer welds in terms of the effect of interlayer thickness on stress, interlayer strain, time-dependent failure, effect of base-metal properties, and effect of interlayer fabrication method. The article concludes with a discussion on multiaxial loading.

You do not currently have access to this content.
Don't already have an account? Register

R.S. Rosen, M.E. Kassner, 1993. "Mechanical Properties of Soft-Interlayer Solid-State Welds", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards