Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Thermal Spray Coatings

By
Herbert Herman
Herbert Herman
State University of New York
Search for other works by this author on:
Robert A. Sulit
Robert A. Sulit
Sulit Engineering
Search for other works by this author on:
Published:
1993
Page range:
1004 - 1009

Abstract

Thermal spray coatings (TSCs) are surface coatings engineered to provide wear-, erosion-, abrasion-, and corrosion-resistant coatings for original equipment manufacture and for the repair and upgrading of in-service equipment. This article presents an overview of five thermal spray processes and the specific flame and arc spray processes used to preserve large steel components and structures. It describes the TSC selection guide and an industrial process procedure guide for applying aluminum and zinc TSCs onto steel.

You do not currently have access to this content.
Don't already have an account? Register

Herbert Herman, Robert A. Sulit, 1993. "Thermal Spray Coatings", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards