Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Evaluation and Quality Control of Brazed Joints

By
Mary B. Vollaro
Mary B. Vollaro
University of Connecticut
Search for other works by this author on:
Jule A. Miller
Jule A. Miller
Consultant
Search for other works by this author on:
Published:
1993
Page range:
1117 - 1123

Abstract

This article outlines the requirements and methods associated with the inspection of brazements. It emphasizes the incorporation of these requirements into the overall quality system. The article reviews the acceptance limits, design limitations, and nondestructive and destructive inspection techniques involved in the brazement inspection. Selected case studies are also provided for further reference.

You do not currently have access to this content.
Don't already have an account? Register

Mary B. Vollaro, Jule A. Miller, 1993. "Evaluation and Quality Control of Brazed Joints", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal