Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Soldering in Electronic Applications

By
Paul T. Vianco
Paul T. Vianco
Sandia National Laboratories
Search for other works by this author on:
Published:
1993
Page range:
985 - 1000

Abstract

Soldering represents the primary method of attaching electronic components, such as resistors, capacitors, or packaged integrated circuits, to either printed wiring board whose defects is minimized by consideration of proper PWB design, device packages, and board assembly. This article discusses the categories that are most important to successful electronic soldering, namely, solders and fluxes selection, nature of base materials and finishes, solder joint design, and solderability testing.

You do not currently have access to this content.
Don't already have an account? Register

Paul T. Vianco, 1993. "Soldering in Electronic Applications", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal