Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Friction Surfacing

By
E.D. Nicholas
E.D. Nicholas
The Welding Institute
Search for other works by this author on:
Published:
1993
Page range:
321 - 323

Abstract

In the friction surfacing process, a rotating consumable is brought into contact with a moving substrate, which results in a deposited layer on the substrate. This article describes the process as well as the equipment used. It also provides information on the applications of the friction surface process.

You do not currently have access to this content.
Don't already have an account? Register

E.D. Nicholas, 1993. "Friction Surfacing", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal