Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Selection of Cobalt-, Titanium-, Zirconium-, and Tantalum-Base Corrosion-Resistant Alloys

By
S.J. Matthews
S.J. Matthews
Haynes International, Inc.
Search for other works by this author on:
Published:
1993
Page range:
598 - 600

Abstract

This article discusses the weldability characteristics of cobalt-base corrosion-resistant (CR) alloys, titanium-base CR alloys, zirconium-base CR alloys, and tantalum-base CR alloys that assist in the selection of suitable alloy and welding method for producing high-quality welds.

You do not currently have access to this content.
Don't already have an account? Register

S.J. Matthews, 1993. "Selection of Cobalt-, Titanium-, Zirconium-, and Tantalum-Base Corrosion-Resistant Alloys", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards