Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Projection Welding[1]

By
Jerry E. Gould
Jerry E. Gould
Edison Welding Institute
Search for other works by this author on:
Published:
1993
Page range:
230 - 237

Abstract

Projection welding (PW) is a variation of resistance welding in which current flow is concentrated at the point of contact with a local geometric extension of one (or both) of the parts being welded. This article discusses the applications of PW generally categorized as either embossed-projection welding or solid-projection welding. Different projection-welding configurations are schematically presented and the common variations of solid-projection welding are described. The article describes equipment used and the process requirement for the PW. The process requirements for projection welding of a range of intermediate-gage low-carbon steels are presented in a table.

You do not currently have access to this content.
Don't already have an account? Register

Jerry E. Gould, 1993. "Projection Welding", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal